Author(s): BENY C.
Date: 11 October 90
file name: ADSAS1.S00 pdf
Recording laboratory: Lab. mixte (BRGM-CNRS- Univ. Orl…ans) de spectrom…trie Raman
References:
2nd file name:
Structural formula: KAlSi3O8
Name: Adularia
Family: Tectosilicates roup: Feldspar
Origin: natural [x] locality: Switzerland synthetic [_] method: P: T:
Solid: crystal [x] powder [_] glass [_]
Fluid: liquid [_] gas [_]
Preparation: Thick section [_] thin section [_] raw sample [x]
Colour:white opaque [_] transparent [x] translucent [_]
Conditions of measurement: room P room T
Polarization setting: PORTO a (c b) a VV [_]; VH [_]; none [_]
Laser: Ar+ 0 = 514.5 nm;
Sample photosensibility: -
Laser power: at laser: 500 mW, at sample:
Raman scattering efficiency: **
Spectral resolution: 5 cm-1
Calibration: Ar+: 77 cm-1
Spectrometer: JOBIN-YVON; model: U1000 macro [x] micro [_] objective:; N.A.: monochannel [x] multichannel [_]
scan rate: cm-1/mn
step: 0.5cm-1
counting time: 1 s
integration time: s
number of scans: 1
accumulations:
Reference:
Crystal system:;
Z:;
space group:
Factor group analysis: : G
Raman shift (cm-1): 1128.5 1099.0 995.0 810.0 796.5 747.5 513.0 474.5 455.0 406.0 368.0 280.5 268.5 219.0 197.0 175.0 162.5 154.0 123.5 110.0 98.0 64.5
Observations: